A4 Stainless Steel Spring (Roll) Pin are supplied to our own published dimensions — this is a trade-series article rather than one covered by a dimensional standard, so confirm the figures against the part you are replacing. The grade provides superior, including marine and chloride environments and is largely non-magnetic; the practical service range is approx. -200 °C to +400 °C, subject to the property class and the joint.
Why Choose A4 Stainless Steel for Spring (Roll) Pin — ISO / DIN (Series 103)
Specified for marine, coastal and chemical applications. For spring (roll) pin — iso / din (series 103), this matters when superior, including marine and chloride environments is the primary requirement.
Mechanical & Physical Properties
| Grade designation | ISO 3506 group A4 (316 / 1.4401), commonly supplied A4-80 |
|---|---|
| Magnetic response | Largely non-magnetic |
| Service temperature | approx. -200 °C to +400 °C, subject to the property class and the joint |
| Corrosion characteristic | Superior, including marine and chloride environments |
Galvanic & Galling Considerations
For stainless spring (roll) pin — iso / din (series 103) the compatibility question is galvanic rather than galling: joined to aluminum or galvanized steel in wet service, stainless drives corrosion of the less-noble metal. Isolate with a coating, sleeve or non-conductive washer where the joint sees moisture. Note also that stainless is softer than hardened carbon steel, so where the part carries a wear or shear duty, check the load against the grade before substituting.
Comparable Grades
For Spring (Roll) Pin — ISO / DIN (Series 103), the alternative stainless grade is A2 (304). The practical dividing line is chlorides: A2 (304) is fine until salt is involved, and A4 (316) exists for the cases where it is — coastal, marine and road-salt service. Neither reaches the strength of a plated class 8.8 or 10.9 fastener.
Using Stainless Fasteners in Aluminum
Stainless steel is more noble than aluminum, so with an electrolyte present — rain, condensation, salt spray — the aluminum becomes the anode and corrodes at the joint. Area ratio decides how bad it gets: a small stainless fastener in a large aluminum section is normally acceptable, a large stainless fastener in thin aluminum is not. Where the joint gets wet, isolate the metals with a coated or nylon washer and a sealant, or specify an aluminum or coated fastener instead.
Sizes of Spring (Roll) Pin — ISO / DIN (Series 103) Available in A4 Stainless Steel
| Nominal diameter (mm) | Length L (mm) | Recommended hole (mm) | Material | Reference standard |
|---|---|---|---|---|
| 2 | 12 | 2.0 | Spring steel | ISO 8752 / DIN 1481 |
| 3 | 16 | 3.0 | Spring steel | ISO 8752 / DIN 1481 |
| 4 | 20 | 4.0 | Spring steel | ISO 8752 / DIN 1481 |
| 5 | 25 | 5.0 | Spring steel | ISO 8752 / DIN 1481 |
| 6 | 32 | 6.0 | Spring steel | ISO 8752 / DIN 1481 |
| 8 | 40 | 8.0 | Spring steel | ISO 8752 / DIN 1481 |
| 10 | 50 | 10.0 | Spring steel | ISO 8752 / DIN 1481 |
| 12 | 63 | 12.0 | Spring steel | ISO 8752 / DIN 1481 |
| 16 | 80 | 16.0 | Spring steel | ISO 8752 / DIN 1481 |
Dimensions are independent of the material: every size above is available in A4 Stainless Steel.
Custom manufacturing · Made to drawing
Need this pin in a grade that is not listed?
A4 Stainless Steel is one of the grades the catalog describes. End form, hardness and surface finish are all variable; the diameter tolerance is the one that decides the process. Made by cold heading or turning.
Minimum order from 2,000 pieces; samples within 7 days of drawing approval.