Grade 12.9 Steel Thin Hex Nut, Fine Pitch

Grade 12.9 Steel Thin Hex Nut, Fine Pitch reference image

Grade 12.9 Steel Thin Hex Nut, Fine Pitch combine the dimensional form of GB/T 6173 / ISO 8675 with the material properties of grade class 12.9: requires plating or black-oxide protection, magnetic, service range up to approx. +300 °C. This page summarizes the grade data, its corrosion behavior in service, the comparable grades, and the sizes supplied.

Why Choose Grade 12.9 Steel for Thin Hex Nut, Fine Pitch — GB/T 6173 / ISO 8675 (Series 056)

The highest common strength class, for high-load machine assembly. For thin hex nut, fine pitch — gb/t 6173 / iso 8675 (series 056), this matters when requires plating or black-oxide protection is the primary requirement.

Mechanical & Physical Properties

Grade designationclass 12.9
Magnetic responseMagnetic
Service temperatureup to approx. +300 °C
Corrosion characteristicRequires plating or black-oxide protection

Galvanic & Galling Considerations

For thin hex nut, fine pitch — gb/t 6173 / iso 8675 (series 056) in steel, the dominant compatibility issue is hydrogen embrittlement at high property classes (10.9 and above) when electroplated. Plating must be followed by an appropriate baking treatment, or a non-electroplated finish (mechanical zinc, zinc flake) should be substituted.

Comparable Grades

For Thin Hex Nut, Fine Pitch — GB/T 6173 / ISO 8675 (Series 056), class 8.8 is the comparable strength step. Move up when the joint preload approaches the proof load of the current class; move down when the joint is over-specified. For corrosion-critical service, switch to stainless A2 or A4.

Sizes of Thin Hex Nut, Fine Pitch — GB/T 6173 / ISO 8675 (Series 056) Available in Grade 12.9 Steel

SizePitch (mm)Width across flats s (mm)Width across corners e (mm)Nut height m (mm)Reference standard
M30.55.56.011.8ISO 4035 / GB/T 6172
M40.77.07.662.2ISO 4035 / GB/T 6172
M50.88.08.792.7ISO 4035 / GB/T 6172
M61.010.011.053.2ISO 4035 / GB/T 6172
M81.2513.014.384.0ISO 4035 / GB/T 6172
M101.516.017.775.0ISO 4035 / GB/T 6172
M121.7518.020.036.0ISO 4035 / GB/T 6172
M142.021.023.367.0ISO 4035 / GB/T 6172
M162.024.026.758.0ISO 4035 / GB/T 6172
M182.527.030.149.0ISO 4035 / GB/T 6172
M202.530.033.5310.0ISO 4035 / GB/T 6172
M243.036.039.9812.0ISO 4035 / GB/T 6172
M303.546.050.8515.0ISO 4035 / GB/T 6172
M364.055.060.7918.0ISO 4035 / GB/T 6172

Technical Drawing

Customize the parameters below — every spec field is editable, and the drawing redraws to match the values you choose. Changing the size will snap the other fields to that size's standard values; you can then override any individual value.

Sends the selected values to the quote form below.

Request a Quote

Adjust the parameters in the drawing above and click "Request this configuration" to send the exact specification straight to this form.

Request a Quotation

Specification
Business Information

Dimensions & Specifications (GB/T 6173 / ISO 8675)

SizePitch (mm)Width across flats s (mm)Width across corners e (mm)Nut height m (mm)Reference standard
M30.55.56.011.8ISO 4035 / GB/T 6172
M40.77.07.662.2ISO 4035 / GB/T 6172
M50.88.08.792.7ISO 4035 / GB/T 6172
M61.010.011.053.2ISO 4035 / GB/T 6172
M81.2513.014.384.0ISO 4035 / GB/T 6172
M101.516.017.775.0ISO 4035 / GB/T 6172
M121.7518.020.036.0ISO 4035 / GB/T 6172
M142.021.023.367.0ISO 4035 / GB/T 6172
M162.024.026.758.0ISO 4035 / GB/T 6172
M182.527.030.149.0ISO 4035 / GB/T 6172
M202.530.033.5310.0ISO 4035 / GB/T 6172
M243.036.039.9812.0ISO 4035 / GB/T 6172
M303.546.050.8515.0ISO 4035 / GB/T 6172
M364.055.060.7918.0ISO 4035 / GB/T 6172

Frequently Asked Questions

Are Grade 12.9 Steel Thin Hex Nut, Fine Pitch — GB/T 6173 / ISO 8675 (Series 056) magnetic?

Grade 12.9 Steel Thin Hex Nut, Fine Pitch — GB/T 6173 / ISO 8675 (Series 056) are magnetic.

What corrosion resistance do Grade 12.9 Steel Thin Hex Nut, Fine Pitch — GB/T 6173 / ISO 8675 (Series 056) offer?

Grade 12.9 Steel Thin Hex Nut, Fine Pitch — GB/T 6173 / ISO 8675 (Series 056) provide requires plating or black-oxide protection with a service range of up to approx. +300 °C.

When should I move from class 12.9 to class 8.8 for Thin Hex Nut, Fine Pitch — GB/T 6173 / ISO 8675 (Series 056)?

Step up to class 8.8 when the joint preload approaches the proof load of the current class. The higher class adds preload at the same diameter, often saving size and weight.

Is Grade 12.9 Steel prone to hydrogen embrittlement?

Class 10.9 and above can be susceptible to hydrogen embrittlement when electroplated. Specify post-plating baking, or use mechanical-zinc / zinc-flake finishes which avoid the cathodic plating step.