Skip to content

Bolts · GB/T 15389 / DIN 938

Grade 8.8 Steel Stud Bolt, Double-End — GB/T 15389 / DIN 938 (Series 092)

Specifying Stud Bolt, Double-End — GB/T 15389 / DIN 938 (Series 092) in Grade 8.8 Steel pairs the dimensional form of Stud Bolt, Double-End — GB/T 15389 / DIN 938 (Series 092) (GB/T 15389 / DIN 938) with the engineering properties of Grade 8.8 Steel. This page explains when to choose the grade, how it behaves in service, and which grades to compare it against.

Why Choose Grade 8.8 Steel for Stud Bolt, Double-End — GB/T 15389 / DIN 938 (Series 092)

The workhorse medium-carbon alloy grade for structural joints. For stud bolt, double-end — gb/t 15389 / din 938 (series 092), this matters when requires plating (zinc) for corrosion protection is the primary requirement.

Mechanical & Physical Properties

Grade designationclass 8.8
Magnetic responseMagnetic
Service temperatureup to approx. +300 °C
Corrosion characteristicRequires plating (zinc) for corrosion protection

Corrosion Behavior in Service

Carbon and alloy steel stud bolt, double-end — gb/t 15389 / din 938 (series 092) require a coating for corrosion protection. Zinc plating (with or without passivation) is the most common; hot-dip galvanizing is used for outdoor structural service; black-oxide is mainly a tarnish-prevention finish for tool-room use.

Galvanic & Galling Considerations

For stud bolt, double-end — gb/t 15389 / din 938 (series 092) in steel, the dominant compatibility issue is hydrogen embrittlement at high property classes (10.9 and above) when electroplated. Plating must be followed by an appropriate baking treatment, or a non-electroplated finish (mechanical zinc, zinc flake) should be substituted.

Sizes of Stud Bolt, Double-End — GB/T 15389 / DIN 938 (Series 092) Available in Grade 8.8 Steel

Thread sizePitch (mm)Length L (mm)Engagement depth bm (mm)MaterialReference standard
M61.0508Cl. 8.8 alloy steelDIN 939 / GB/T 901
M81.256010Cl. 8.8 alloy steelDIN 939 / GB/T 901
M101.58015Cl. 8.8 alloy steelDIN 939 / GB/T 901
M121.7510018Cl. 8.8 alloy steelDIN 939 / GB/T 901
M142.012021Cl. 8.8 alloy steelDIN 939 / GB/T 901
M162.015024Cl. 8.8 alloy steelDIN 939 / GB/T 901
M202.518030Cl. 8.8 alloy steelDIN 939 / GB/T 901
M243.020036Cl. 8.8 alloy steelDIN 939 / GB/T 901
M303.524045Cl. 8.8 alloy steelDIN 939 / GB/T 901
M364.028054Cl. 8.8 alloy steelDIN 939 / GB/T 901

Technical Drawing

Customize the parameters below — every spec field is editable, and the drawing redraws to match the values you choose. Changing the size will snap the other fields to that size's standard values; you can then override any individual value.

Sends the selected values to the quote form below.

Request a Quote

Adjust the parameters in the drawing above and click "Request this configuration" to send the exact specification straight to this form.

Request a Quotation

Specification
Business Information

Dimensions & Specifications (GB/T 15389 / DIN 938)

Thread sizePitch (mm)Length L (mm)Engagement depth bm (mm)MaterialReference standard
M61.0508Cl. 8.8 alloy steelDIN 939 / GB/T 901
M81.256010Cl. 8.8 alloy steelDIN 939 / GB/T 901
M101.58015Cl. 8.8 alloy steelDIN 939 / GB/T 901
M121.7510018Cl. 8.8 alloy steelDIN 939 / GB/T 901
M142.012021Cl. 8.8 alloy steelDIN 939 / GB/T 901
M162.015024Cl. 8.8 alloy steelDIN 939 / GB/T 901
M202.518030Cl. 8.8 alloy steelDIN 939 / GB/T 901
M243.020036Cl. 8.8 alloy steelDIN 939 / GB/T 901
M303.524045Cl. 8.8 alloy steelDIN 939 / GB/T 901
M364.028054Cl. 8.8 alloy steelDIN 939 / GB/T 901

Frequently Asked Questions

Are Grade 8.8 Steel Stud Bolt, Double-End — GB/T 15389 / DIN 938 (Series 092) magnetic?

Grade 8.8 Steel Stud Bolt, Double-End — GB/T 15389 / DIN 938 (Series 092) are magnetic.

What corrosion resistance do Grade 8.8 Steel Stud Bolt, Double-End — GB/T 15389 / DIN 938 (Series 092) offer?

Grade 8.8 Steel Stud Bolt, Double-End — GB/T 15389 / DIN 938 (Series 092) provide requires plating (zinc) for corrosion protection with a service range of up to approx. +300 °C.

When should I move from class 8.8 to class 10.9 / 12.9 for Stud Bolt, Double-End — GB/T 15389 / DIN 938 (Series 092)?

Step up to class 10.9 / 12.9 when the joint preload approaches the proof load of the current class. The higher class adds preload at the same diameter, often saving size and weight.

Is Grade 8.8 Steel prone to hydrogen embrittlement?

Class 10.9 and above can be susceptible to hydrogen embrittlement when electroplated. Specify post-plating baking, or use mechanical-zinc / zinc-flake finishes which avoid the cathodic plating step.