Grade 8.8 Steel Thin Hex Nut

Grade 8.8 Steel Thin Hex Nut reference image

Grade 8.8 Steel (class 8.8) is the workhorse medium-carbon alloy grade for structural joints. When thin hex nut are specified in this grade, the dimensions remain per GB/T 901 / DIN 939; the material determines corrosion behavior (requires plating (zinc) for corrosion protection) and the service temperature range (up to approx. +300 °C). Both are covered below with the size table.

Why Choose Grade 8.8 Steel for Thin Hex Nut — GB/T 901 / DIN 939 (Series 094)

The workhorse medium-carbon alloy grade for structural joints. For thin hex nut — gb/t 901 / din 939 (series 094), this matters when requires plating (zinc) for corrosion protection is the primary requirement.

Mechanical & Physical Properties

Grade designationclass 8.8
Magnetic responseMagnetic
Service temperatureup to approx. +300 °C
Corrosion characteristicRequires plating (zinc) for corrosion protection

Galvanic & Galling Considerations

For thin hex nut — gb/t 901 / din 939 (series 094) in steel, the dominant compatibility issue is hydrogen embrittlement at high property classes (10.9 and above) when electroplated. Plating must be followed by an appropriate baking treatment, or a non-electroplated finish (mechanical zinc, zinc flake) should be substituted.

Comparable Grades

For Thin Hex Nut — GB/T 901 / DIN 939 (Series 094), class 10.9 or 12.9 is the comparable strength step. Move up when the joint preload approaches the proof load of the current class; move down when the joint is over-specified. For corrosion-critical service, switch to stainless A2 or A4.

Sizes of Thin Hex Nut — GB/T 901 / DIN 939 (Series 094) Available in Grade 8.8 Steel

SizePitch (mm)Width across flats s (mm)Width across corners e (mm)Nut height m (mm)Reference standard
M30.55.56.011.8ISO 4035 / GB/T 6172
M40.77.07.662.2ISO 4035 / GB/T 6172
M50.88.08.792.7ISO 4035 / GB/T 6172
M61.010.011.053.2ISO 4035 / GB/T 6172
M81.2513.014.384.0ISO 4035 / GB/T 6172
M101.516.017.775.0ISO 4035 / GB/T 6172
M121.7518.020.036.0ISO 4035 / GB/T 6172
M142.021.023.367.0ISO 4035 / GB/T 6172
M162.024.026.758.0ISO 4035 / GB/T 6172
M182.527.030.149.0ISO 4035 / GB/T 6172
M202.530.033.5310.0ISO 4035 / GB/T 6172
M243.036.039.9812.0ISO 4035 / GB/T 6172
M303.546.050.8515.0ISO 4035 / GB/T 6172
M364.055.060.7918.0ISO 4035 / GB/T 6172

Technical Drawing

Customize the parameters below — every spec field is editable, and the drawing redraws to match the values you choose. Changing the size will snap the other fields to that size's standard values; you can then override any individual value.

Sends the selected values to the quote form below.

Request a Quote

Adjust the parameters in the drawing above and click "Request this configuration" to send the exact specification straight to this form.

Request a Quotation

Specification
Business Information

Dimensions & Specifications (GB/T 901 / DIN 939)

SizePitch (mm)Width across flats s (mm)Width across corners e (mm)Nut height m (mm)Reference standard
M30.55.56.011.8ISO 4035 / GB/T 6172
M40.77.07.662.2ISO 4035 / GB/T 6172
M50.88.08.792.7ISO 4035 / GB/T 6172
M61.010.011.053.2ISO 4035 / GB/T 6172
M81.2513.014.384.0ISO 4035 / GB/T 6172
M101.516.017.775.0ISO 4035 / GB/T 6172
M121.7518.020.036.0ISO 4035 / GB/T 6172
M142.021.023.367.0ISO 4035 / GB/T 6172
M162.024.026.758.0ISO 4035 / GB/T 6172
M182.527.030.149.0ISO 4035 / GB/T 6172
M202.530.033.5310.0ISO 4035 / GB/T 6172
M243.036.039.9812.0ISO 4035 / GB/T 6172
M303.546.050.8515.0ISO 4035 / GB/T 6172
M364.055.060.7918.0ISO 4035 / GB/T 6172

Frequently Asked Questions

What corrosion resistance do Grade 8.8 Steel Thin Hex Nut — GB/T 901 / DIN 939 (Series 094) offer?

Grade 8.8 Steel Thin Hex Nut — GB/T 901 / DIN 939 (Series 094) provide requires plating (zinc) for corrosion protection with a service range of up to approx. +300 °C.

When should I move from class 8.8 to class 10.9 / 12.9 for Thin Hex Nut — GB/T 901 / DIN 939 (Series 094)?

Step up to class 10.9 / 12.9 when the joint preload approaches the proof load of the current class. The higher class adds preload at the same diameter, often saving size and weight.

Is Grade 8.8 Steel prone to hydrogen embrittlement?

Class 10.9 and above can be susceptible to hydrogen embrittlement when electroplated. Specify post-plating baking, or use mechanical-zinc / zinc-flake finishes which avoid the cathodic plating step.

Which finish is best for outdoor Thin Hex Nut — GB/T 901 / DIN 939 (Series 094)?

For outdoor service in steel, hot-dip galvanizing gives the longest life; zinc-flake (Geomet/Delta-Tone family) gives a thinner film with excellent salt-spray performance; standard zinc plating is the lowest-cost option for general indoor / shielded outdoor use.