Grade 8.8 Steel Stud — GB/T 15389 / DIN 939 (Series 096)

Grade 8.8 Steel Stud — GB/T 15389 / DIN 939 (Series 096) pairs the standard GB/T 15389 / DIN 939 with a Grade 8.8 Steel base material. The sections below cover why engineers select this grade for stud — gb/t 15389 / din 939 (series 096), its corrosion and temperature behavior, and the sizes available.

Why Choose Grade 8.8 Steel for Stud — GB/T 15389 / DIN 939 (Series 096)

The workhorse medium-carbon alloy grade for structural joints. For stud — gb/t 15389 / din 939 (series 096), this matters when requires plating (zinc) for corrosion protection is the primary requirement.

Mechanical & Physical Properties

Grade designationclass 8.8
Magnetic responseMagnetic
Service temperatureup to approx. +300 °C
Corrosion characteristicRequires plating (zinc) for corrosion protection

Corrosion Behavior in Service

Carbon and alloy steel stud — gb/t 15389 / din 939 (series 096) require a coating for corrosion protection. Zinc plating (with or without passivation) is the most common; hot-dip galvanizing is used for outdoor structural service; black-oxide is mainly a tarnish-prevention finish for tool-room use.

Comparable Grades

For Stud — GB/T 15389 / DIN 939 (Series 096), class 10.9 or 12.9 is the comparable strength step. Move up when the joint preload approaches the proof load of the current class; move down when the joint is over-specified. For corrosion-critical service, switch to stainless A2 or A4.

Sizes of Stud — GB/T 15389 / DIN 939 (Series 096) Available in Grade 8.8 Steel

Thread sizePitch (mm)Length L (mm)Engagement depth bm (mm)MaterialReference standard
M61.0508Cl. 8.8 alloy steelDIN 939 / GB/T 901
M81.256010Cl. 8.8 alloy steelDIN 939 / GB/T 901
M101.58015Cl. 8.8 alloy steelDIN 939 / GB/T 901
M121.7510018Cl. 8.8 alloy steelDIN 939 / GB/T 901
M142.012021Cl. 8.8 alloy steelDIN 939 / GB/T 901
M162.015024Cl. 8.8 alloy steelDIN 939 / GB/T 901
M202.518030Cl. 8.8 alloy steelDIN 939 / GB/T 901
M243.020036Cl. 8.8 alloy steelDIN 939 / GB/T 901
M303.524045Cl. 8.8 alloy steelDIN 939 / GB/T 901
M364.028054Cl. 8.8 alloy steelDIN 939 / GB/T 901

Technical Drawing

Customize the parameters below — every spec field is editable, and the drawing redraws to match the values you choose. Changing the size will snap the other fields to that size's standard values; you can then override any individual value.

Sends the selected values to the quote form below.

Request a Quote

Adjust the parameters in the drawing above and click "Request this configuration" to send the exact specification straight to this form.

Request a Quotation

Specification
Business Information

Dimensions & Specifications (GB/T 15389 / DIN 939)

Thread sizePitch (mm)Length L (mm)Engagement depth bm (mm)MaterialReference standard
M61.0508Cl. 8.8 alloy steelDIN 939 / GB/T 901
M81.256010Cl. 8.8 alloy steelDIN 939 / GB/T 901
M101.58015Cl. 8.8 alloy steelDIN 939 / GB/T 901
M121.7510018Cl. 8.8 alloy steelDIN 939 / GB/T 901
M142.012021Cl. 8.8 alloy steelDIN 939 / GB/T 901
M162.015024Cl. 8.8 alloy steelDIN 939 / GB/T 901
M202.518030Cl. 8.8 alloy steelDIN 939 / GB/T 901
M243.020036Cl. 8.8 alloy steelDIN 939 / GB/T 901
M303.524045Cl. 8.8 alloy steelDIN 939 / GB/T 901
M364.028054Cl. 8.8 alloy steelDIN 939 / GB/T 901

Frequently Asked Questions

When should I move from class 8.8 to class 10.9 / 12.9 for Stud — GB/T 15389 / DIN 939 (Series 096)?

Step up to class 10.9 / 12.9 when the joint preload approaches the proof load of the current class. The higher class adds preload at the same diameter, often saving size and weight.

Is Grade 8.8 Steel prone to hydrogen embrittlement?

Class 10.9 and above can be susceptible to hydrogen embrittlement when electroplated. Specify post-plating baking, or use mechanical-zinc / zinc-flake finishes which avoid the cathodic plating step.

Which finish is best for outdoor Stud — GB/T 15389 / DIN 939 (Series 096)?

For outdoor service in steel, hot-dip galvanizing gives the longest life; zinc-flake (Geomet/Delta-Tone family) gives a thinner film with excellent salt-spray performance; standard zinc plating is the lowest-cost option for general indoor / shielded outdoor use.

What's the service temperature limit for Grade 8.8 Steel?

The practical service range is up to approx. +300 °C.