Split Cotter Pin manufactured in Grade 8.8 Steel (class 8.8) are dimensioned to ISO / DIN. The sections below give the mechanical and physical properties of the grade, its behavior in corrosive and elevated-temperature service, and the full size table.

Why Choose Grade 8.8 Steel for Split Cotter Pin — ISO / DIN (Series 102)

The workhorse medium-carbon alloy grade for structural joints. For split cotter pin — iso / din (series 102), this matters when requires plating (zinc) for corrosion protection is the primary requirement.

Mechanical & Physical Properties

Grade designationclass 8.8
Magnetic responseMagnetic
Service temperatureup to approx. +300 °C
Corrosion characteristicRequires plating (zinc) for corrosion protection

Corrosion Behavior in Service

Carbon and alloy steel split cotter pin — iso / din (series 102) require a coating for corrosion protection. Zinc plating (with or without passivation) is the most common; hot-dip galvanizing is used for outdoor structural service; black-oxide is mainly a tarnish-prevention finish for tool-room use.

Comparable Grades

For Split Cotter Pin — ISO / DIN (Series 102), class 10.9 or 12.9 is the comparable strength step. Move up when the joint preload approaches the proof load of the current class; move down when the joint is over-specified. For corrosion-critical service, switch to stainless A2 or A4.

Sizes of Split Cotter Pin — ISO / DIN (Series 102) Available in Grade 8.8 Steel

Nominal diameter (mm)Length L (mm)MaterialReference standard
1.016Carbon steelISO 1234 / GB/T 91
1.220Carbon steelISO 1234 / GB/T 91
1.625Carbon steelISO 1234 / GB/T 91
2.032Carbon steelISO 1234 / GB/T 91
2.540Carbon steelISO 1234 / GB/T 91
3.250Carbon steelISO 1234 / GB/T 91
4.063Carbon steelISO 1234 / GB/T 91
5.080Carbon steelISO 1234 / GB/T 91
6.3100Carbon steelISO 1234 / GB/T 91
8.0125Carbon steelISO 1234 / GB/T 91

Technical Drawing

Customize the parameters below — every spec field is editable, and the drawing redraws to match the values you choose. Changing the size will snap the other fields to that size's standard values; you can then override any individual value.

Sends the selected values to the quote form below.

Request a Quote

Adjust the parameters in the drawing above and click "Request this configuration" to send the exact specification straight to this form.

Request a Quotation

Specification
Business Information

Dimensions & Specifications (ISO / DIN)

Nominal diameter (mm)Length L (mm)MaterialReference standard
1.016Carbon steelISO 1234 / GB/T 91
1.220Carbon steelISO 1234 / GB/T 91
1.625Carbon steelISO 1234 / GB/T 91
2.032Carbon steelISO 1234 / GB/T 91
2.540Carbon steelISO 1234 / GB/T 91
3.250Carbon steelISO 1234 / GB/T 91
4.063Carbon steelISO 1234 / GB/T 91
5.080Carbon steelISO 1234 / GB/T 91
6.3100Carbon steelISO 1234 / GB/T 91
8.0125Carbon steelISO 1234 / GB/T 91

Frequently Asked Questions

Is Grade 8.8 Steel prone to hydrogen embrittlement?

Class 10.9 and above can be susceptible to hydrogen embrittlement when electroplated. Specify post-plating baking, or use mechanical-zinc / zinc-flake finishes which avoid the cathodic plating step.

Which finish is best for outdoor Split Cotter Pin — ISO / DIN (Series 102)?

For outdoor service in steel, hot-dip galvanizing gives the longest life; zinc-flake (Geomet/Delta-Tone family) gives a thinner film with excellent salt-spray performance; standard zinc plating is the lowest-cost option for general indoor / shielded outdoor use.

What's the service temperature limit for Grade 8.8 Steel?

The practical service range is up to approx. +300 °C.

Can Grade 8.8 Steel replace stainless steel structurally?

No — stainless A2/A4 cannot match class 10.9 / 12.9 strength. Stainless is selected for corrosion, not raw strength.

How do I request a quotation?

Use the technical drawing on this page to pick the exact configuration, then submit it with the quote form. We respond within one business day.