Grade 8.8 Steel Hex Bolt — GB/T 5783 / ISO 4017 (Series 010)

Specifying Hex Bolt — GB/T 5783 / ISO 4017 (Series 010) in Grade 8.8 Steel pairs the dimensional form of Hex Bolt — GB/T 5783 / ISO 4017 (Series 010) (GB/T 5783 / ISO 4017) with the engineering properties of Grade 8.8 Steel. This page explains when to choose the grade, how it behaves in service, and which grades to compare it against.

Why Choose Grade 8.8 Steel for Hex Bolt — GB/T 5783 / ISO 4017 (Series 010)

The workhorse medium-carbon alloy grade for structural joints. For hex bolt — gb/t 5783 / iso 4017 (series 010), this matters when requires plating (zinc) for corrosion protection is the primary requirement.

Mechanical & Physical Properties

Grade designationclass 8.8
Magnetic responseMagnetic
Service temperatureup to approx. +300 °C
Corrosion characteristicRequires plating (zinc) for corrosion protection

Corrosion Behavior in Service

Carbon and alloy steel hex bolt — gb/t 5783 / iso 4017 (series 010) require a coating for corrosion protection. Zinc plating (with or without passivation) is the most common; hot-dip galvanizing is used for outdoor structural service; black-oxide is mainly a tarnish-prevention finish for tool-room use.

Galvanic & Galling Considerations

For hex bolt — gb/t 5783 / iso 4017 (series 010) in steel, the dominant compatibility issue is hydrogen embrittlement at high property classes (10.9 and above) when electroplated. Plating must be followed by an appropriate baking treatment, or a non-electroplated finish (mechanical zinc, zinc flake) should be substituted.

Sizes of Hex Bolt — GB/T 5783 / ISO 4017 (Series 010) Available in Grade 8.8 Steel

SizePitch (mm)Nominal diameter d (mm)Length L (mm)Width across flats s (mm)Width across corners e (mm)Head height k (mm)
M30.53205.56.012.0
M40.74257.07.662.8
M50.85308.08.793.5
M61.064010.011.054.0
M81.2585013.014.385.3
M101.5106016.017.776.4
M121.75128018.020.037.5
M142.0148021.023.368.8
M162.01610024.026.7510.0
M182.51810027.030.1411.5
M202.52012030.033.5312.5
M243.02415036.039.9815.0
M303.53018046.050.8518.7
M364.03620055.060.7922.5

Technical Drawing

Customize the parameters below — every spec field is editable, and the drawing redraws to match the values you choose. Changing the size will snap the other fields to that size's standard values; you can then override any individual value.

Sends the selected values to the quote form below.

Request a Quote

Adjust the parameters in the drawing above and click "Request this configuration" to send the exact specification straight to this form.

Request a Quotation

Specification
Business Information

Dimensions & Specifications (GB/T 5783 / ISO 4017)

SizePitch (mm)Nominal diameter d (mm)Length L (mm)Width across flats s (mm)Width across corners e (mm)Head height k (mm)
M30.53205.56.012.0
M40.74257.07.662.8
M50.85308.08.793.5
M61.064010.011.054.0
M81.2585013.014.385.3
M101.5106016.017.776.4
M121.75128018.020.037.5
M142.0148021.023.368.8
M162.01610024.026.7510.0
M182.51810027.030.1411.5
M202.52012030.033.5312.5
M243.02415036.039.9815.0
M303.53018046.050.8518.7
M364.03620055.060.7922.5

Frequently Asked Questions

When should I move from class 8.8 to class 10.9 / 12.9 for Hex Bolt — GB/T 5783 / ISO 4017 (Series 010)?

Step up to class 10.9 / 12.9 when the joint preload approaches the proof load of the current class. The higher class adds preload at the same diameter, often saving size and weight.

Is Grade 8.8 Steel prone to hydrogen embrittlement?

Class 10.9 and above can be susceptible to hydrogen embrittlement when electroplated. Specify post-plating baking, or use mechanical-zinc / zinc-flake finishes which avoid the cathodic plating step.

Which finish is best for outdoor Hex Bolt — GB/T 5783 / ISO 4017 (Series 010)?

For outdoor service in steel, hot-dip galvanizing gives the longest life; zinc-flake (Geomet/Delta-Tone family) gives a thinner film with excellent salt-spray performance; standard zinc plating is the lowest-cost option for general indoor / shielded outdoor use.

What's the service temperature limit for Grade 8.8 Steel?

The practical service range is up to approx. +300 °C.

How do I request a quotation?

Use the technical drawing on this page to pick the exact configuration, then submit it with the quote form. We respond within one business day.