Screws · GB/T 819.1 / ISO 7046

Grade 8.8 Steel Phillips Countersunk Machine Screw — GB/T 819.1 / ISO 7046 (Series 030)

For Phillips Countersunk Machine Screw — GB/T 819.1 / ISO 7046 (Series 030) in Grade 8.8 Steel, the controlling decisions are corrosion, strength and service temperature. This guide summarizes those three for Grade 8.8 Steel Phillips Countersunk Machine Screw — GB/T 819.1 / ISO 7046 (Series 030) and lists every size we supply.

Why Choose Grade 8.8 Steel for Phillips Countersunk Machine Screw — GB/T 819.1 / ISO 7046 (Series 030)

The workhorse medium-carbon alloy grade for structural joints. For phillips countersunk machine screw — gb/t 819.1 / iso 7046 (series 030), this matters when requires plating (zinc) for corrosion protection is the primary requirement.

Mechanical & Physical Properties

Grade designationclass 8.8
Magnetic responseMagnetic
Service temperatureup to approx. +300 °C
Corrosion characteristicRequires plating (zinc) for corrosion protection

Corrosion Behavior in Service

Carbon and alloy steel phillips countersunk machine screw — gb/t 819.1 / iso 7046 (series 030) require a coating for corrosion protection. Zinc plating (with or without passivation) is the most common; hot-dip galvanizing is used for outdoor structural service; black-oxide is mainly a tarnish-prevention finish for tool-room use.

Comparable Grades

For Phillips Countersunk Machine Screw — GB/T 819.1 / ISO 7046 (Series 030), class 10.9 or 12.9 is the comparable strength step. Move up when the joint preload approaches the proof load of the current class; move down when the joint is over-specified. For corrosion-critical service, switch to stainless A2 or A4.

Sizes of Phillips Countersunk Machine Screw — GB/T 819.1 / ISO 7046 (Series 030) Available in Grade 8.8 Steel

SizePitch (mm)Length L (mm)Head diameter dk (mm)Head height k (mm)Cross recessCountersink angle (deg)Reference standard
M30.5205.61.65PH190ISO 7046 / GB/T 819
M40.7257.52.2PH290ISO 7046 / GB/T 819
M50.8309.22.5PH290ISO 7046 / GB/T 819
M61.04011.03.0PH390ISO 7046 / GB/T 819
M81.255014.54.0PH390ISO 7046 / GB/T 819
M101.56018.05.0PH490ISO 7046 / GB/T 819
M121.758022.06.0PH490ISO 7046 / GB/T 819
M142.08025.07.0PH490ISO 7046 / GB/T 819
M162.010029.08.0PH490ISO 7046 / GB/T 819
M182.510033.09.0PH490ISO 7046 / GB/T 819
M202.512036.510.0PH490ISO 7046 / GB/T 819
M243.015043.512.0PH490ISO 7046 / GB/T 819

Technical Drawing

Customize the parameters below — every spec field is editable, and the drawing redraws to match the values you choose. Changing the size will snap the other fields to that size's standard values; you can then override any individual value.

Sends the selected values to the quote form below.

Request a Quote

Adjust the parameters in the drawing above and click "Request this configuration" to send the exact specification straight to this form.

Request a Quotation

Specification
Business Information

Dimensions & Specifications (GB/T 819.1 / ISO 7046)

SizePitch (mm)Length L (mm)Head diameter dk (mm)Head height k (mm)Cross recessCountersink angle (deg)Reference standard
M30.5205.61.65PH190ISO 7046 / GB/T 819
M40.7257.52.2PH290ISO 7046 / GB/T 819
M50.8309.22.5PH290ISO 7046 / GB/T 819
M61.04011.03.0PH390ISO 7046 / GB/T 819
M81.255014.54.0PH390ISO 7046 / GB/T 819
M101.56018.05.0PH490ISO 7046 / GB/T 819
M121.758022.06.0PH490ISO 7046 / GB/T 819
M142.08025.07.0PH490ISO 7046 / GB/T 819
M162.010029.08.0PH490ISO 7046 / GB/T 819
M182.510033.09.0PH490ISO 7046 / GB/T 819
M202.512036.510.0PH490ISO 7046 / GB/T 819
M243.015043.512.0PH490ISO 7046 / GB/T 819

Frequently Asked Questions

Is Grade 8.8 Steel prone to hydrogen embrittlement?

Class 10.9 and above can be susceptible to hydrogen embrittlement when electroplated. Specify post-plating baking, or use mechanical-zinc / zinc-flake finishes which avoid the cathodic plating step.

Which finish is best for outdoor Phillips Countersunk Machine Screw — GB/T 819.1 / ISO 7046 (Series 030)?

For outdoor service in steel, hot-dip galvanizing gives the longest life; zinc-flake (Geomet/Delta-Tone family) gives a thinner film with excellent salt-spray performance; standard zinc plating is the lowest-cost option for general indoor / shielded outdoor use.

What's the service temperature limit for Grade 8.8 Steel?

The practical service range is up to approx. +300 °C.

Can Grade 8.8 Steel replace stainless steel structurally?

No — stainless A2/A4 cannot match class 10.9 / 12.9 strength. Stainless is selected for corrosion, not raw strength.