Grade 8.8 Steel Rod End Bearing — ISO / DIN (Series 108)

Specifying Rod End Bearing — ISO / DIN (Series 108) in Grade 8.8 Steel pairs the dimensional form of Rod End Bearing — ISO / DIN (Series 108) (ISO / DIN) with the engineering properties of Grade 8.8 Steel. This page explains when to choose the grade, how it behaves in service, and which grades to compare it against.

Why Choose Grade 8.8 Steel for Rod End Bearing — ISO / DIN (Series 108)

The workhorse medium-carbon alloy grade for structural joints. For rod end bearing — iso / din (series 108), this matters when requires plating (zinc) for corrosion protection is the primary requirement.

Mechanical & Physical Properties

Grade designationclass 8.8
Magnetic responseMagnetic
Service temperatureup to approx. +300 °C
Corrosion characteristicRequires plating (zinc) for corrosion protection

Galvanic & Galling Considerations

For rod end bearing — iso / din (series 108) in steel, the dominant compatibility issue is hydrogen embrittlement at high property classes (10.9 and above) when electroplated. Plating must be followed by an appropriate baking treatment, or a non-electroplated finish (mechanical zinc, zinc flake) should be substituted.

Comparable Grades

For Rod End Bearing — ISO / DIN (Series 108), class 10.9 or 12.9 is the comparable strength step. Move up when the joint preload approaches the proof load of the current class; move down when the joint is over-specified. For corrosion-critical service, switch to stainless A2 or A4.

Sizes of Rod End Bearing — ISO / DIN (Series 108) Available in Grade 8.8 Steel

Bore d (mm)Thread sizePitch (mm)Total length (mm)Hex width (mm)Static load Cor (kN)Reference standard
5M50.84082.2DIN ISO 12240 / GB/T 9163
6M61.046103.0DIN ISO 12240 / GB/T 9163
8M81.2557125.0DIN ISO 12240 / GB/T 9163
10M101.571148.0DIN ISO 12240 / GB/T 9163
12M121.75841712.0DIN ISO 12240 / GB/T 9163
16M162.01052221.0DIN ISO 12240 / GB/T 9163
20M202.51312733.0DIN ISO 12240 / GB/T 9163
25M243.01603252.0DIN ISO 12240 / GB/T 9163

Technical Drawing

Customize the parameters below — every spec field is editable, and the drawing redraws to match the values you choose. Changing the size will snap the other fields to that size's standard values; you can then override any individual value.

Sends the selected values to the quote form below.

Request a Quote

Adjust the parameters in the drawing above and click "Request this configuration" to send the exact specification straight to this form.

Request a Quotation

Specification
Business Information

Dimensions & Specifications (ISO / DIN)

Bore d (mm)Thread sizePitch (mm)Total length (mm)Hex width (mm)Static load Cor (kN)Reference standard
5M50.84082.2DIN ISO 12240 / GB/T 9163
6M61.046103.0DIN ISO 12240 / GB/T 9163
8M81.2557125.0DIN ISO 12240 / GB/T 9163
10M101.571148.0DIN ISO 12240 / GB/T 9163
12M121.75841712.0DIN ISO 12240 / GB/T 9163
16M162.01052221.0DIN ISO 12240 / GB/T 9163
20M202.51312733.0DIN ISO 12240 / GB/T 9163
25M243.01603252.0DIN ISO 12240 / GB/T 9163

Frequently Asked Questions

What corrosion resistance do Grade 8.8 Steel Rod End Bearing — ISO / DIN (Series 108) offer?

Grade 8.8 Steel Rod End Bearing — ISO / DIN (Series 108) provide requires plating (zinc) for corrosion protection with a service range of up to approx. +300 °C.

When should I move from class 8.8 to class 10.9 / 12.9 for Rod End Bearing — ISO / DIN (Series 108)?

Step up to class 10.9 / 12.9 when the joint preload approaches the proof load of the current class. The higher class adds preload at the same diameter, often saving size and weight.

Is Grade 8.8 Steel prone to hydrogen embrittlement?

Class 10.9 and above can be susceptible to hydrogen embrittlement when electroplated. Specify post-plating baking, or use mechanical-zinc / zinc-flake finishes which avoid the cathodic plating step.

Which finish is best for outdoor Rod End Bearing — ISO / DIN (Series 108)?

For outdoor service in steel, hot-dip galvanizing gives the longest life; zinc-flake (Geomet/Delta-Tone family) gives a thinner film with excellent salt-spray performance; standard zinc plating is the lowest-cost option for general indoor / shielded outdoor use.