Grade 8.8 Steel Retaining Ring (Circlip) — ISO / DIN (Series 151)

Grade 8.8 Steel Retaining Ring (Circlip) — ISO / DIN (Series 151) pairs the standard ISO / DIN with a Grade 8.8 Steel base material. The sections below cover why engineers select this grade for retaining ring (circlip) — iso / din (series 151), its corrosion and temperature behavior, and the sizes available.

Why Choose Grade 8.8 Steel for Retaining Ring (Circlip) — ISO / DIN (Series 151)

The workhorse medium-carbon alloy grade for structural joints. For retaining ring (circlip) — iso / din (series 151), this matters when requires plating (zinc) for corrosion protection is the primary requirement.

Mechanical & Physical Properties

Grade designationclass 8.8
Magnetic responseMagnetic
Service temperatureup to approx. +300 °C
Corrosion characteristicRequires plating (zinc) for corrosion protection

Corrosion Behavior in Service

Carbon and alloy steel retaining ring (circlip) — iso / din (series 151) require a coating for corrosion protection. Zinc plating (with or without passivation) is the most common; hot-dip galvanizing is used for outdoor structural service; black-oxide is mainly a tarnish-prevention finish for tool-room use.

Comparable Grades

For Retaining Ring (Circlip) — ISO / DIN (Series 151), class 10.9 or 12.9 is the comparable strength step. Move up when the joint preload approaches the proof load of the current class; move down when the joint is over-specified. For corrosion-critical service, switch to stainless A2 or A4.

Sizes of Retaining Ring (Circlip) — ISO / DIN (Series 151) Available in Grade 8.8 Steel

Nominal diameter (mm)Ring diameter d1 (mm)Groove diameter d2 (mm)Thickness s (mm)TypeReference standard
87.47.10.8ExternalDIN 471 / GB/T 894
109.39.01.0ExternalDIN 471 / GB/T 894
1211.110.81.0ExternalDIN 471 / GB/T 894
1615.014.71.0ExternalDIN 471 / GB/T 894
2019.018.71.2ExternalDIN 471 / GB/T 894
2523.923.61.2ExternalDIN 471 / GB/T 894
3028.928.61.5ExternalDIN 471 / GB/T 894
4038.538.21.75ExternalDIN 471 / GB/T 894
5048.548.22.0ExternalDIN 471 / GB/T 894
6058.358.02.0ExternalDIN 471 / GB/T 894
8078.077.72.5ExternalDIN 471 / GB/T 894
10098.097.73.0ExternalDIN 471 / GB/T 894

Technical Drawing

Customize the parameters below — every spec field is editable, and the drawing redraws to match the values you choose. Changing the size will snap the other fields to that size's standard values; you can then override any individual value.

Sends the selected values to the quote form below.

Request a Quote

Adjust the parameters in the drawing above and click "Request this configuration" to send the exact specification straight to this form.

Request a Quotation

Specification
Business Information

Dimensions & Specifications (ISO / DIN)

Nominal diameter (mm)Ring diameter d1 (mm)Groove diameter d2 (mm)Thickness s (mm)TypeReference standard
87.47.10.8ExternalDIN 471 / GB/T 894
109.39.01.0ExternalDIN 471 / GB/T 894
1211.110.81.0ExternalDIN 471 / GB/T 894
1615.014.71.0ExternalDIN 471 / GB/T 894
2019.018.71.2ExternalDIN 471 / GB/T 894
2523.923.61.2ExternalDIN 471 / GB/T 894
3028.928.61.5ExternalDIN 471 / GB/T 894
4038.538.21.75ExternalDIN 471 / GB/T 894
5048.548.22.0ExternalDIN 471 / GB/T 894
6058.358.02.0ExternalDIN 471 / GB/T 894
8078.077.72.5ExternalDIN 471 / GB/T 894
10098.097.73.0ExternalDIN 471 / GB/T 894

Frequently Asked Questions

When should I move from class 8.8 to class 10.9 / 12.9 for Retaining Ring (Circlip) — ISO / DIN (Series 151)?

Step up to class 10.9 / 12.9 when the joint preload approaches the proof load of the current class. The higher class adds preload at the same diameter, often saving size and weight.

Is Grade 8.8 Steel prone to hydrogen embrittlement?

Class 10.9 and above can be susceptible to hydrogen embrittlement when electroplated. Specify post-plating baking, or use mechanical-zinc / zinc-flake finishes which avoid the cathodic plating step.

Which finish is best for outdoor Retaining Ring (Circlip) — ISO / DIN (Series 151)?

For outdoor service in steel, hot-dip galvanizing gives the longest life; zinc-flake (Geomet/Delta-Tone family) gives a thinner film with excellent salt-spray performance; standard zinc plating is the lowest-cost option for general indoor / shielded outdoor use.

What's the service temperature limit for Grade 8.8 Steel?

The practical service range is up to approx. +300 °C.