Skip to content

Nuts · GB/T 6172.1 / ISO 4035

Grade 12.9 Steel Thin Hex Nut — GB/T 6172.1 / ISO 4035 (Series 055)

When Thin Hex Nut — GB/T 6172.1 / ISO 4035 (Series 055) are required in Grade 12.9 Steel, the alternative grades and the trade-offs between them matter as much as the dimensions. This page covers both, plus mechanical and corrosion data.

Why Choose Grade 12.9 Steel for Thin Hex Nut — GB/T 6172.1 / ISO 4035 (Series 055)

The highest common strength class, for high-load machine assembly. For thin hex nut — gb/t 6172.1 / iso 4035 (series 055), this matters when requires plating or black-oxide protection is the primary requirement.

Mechanical & Physical Properties

Grade designationclass 12.9
Magnetic responseMagnetic
Service temperatureup to approx. +300 °C
Corrosion characteristicRequires plating or black-oxide protection

Corrosion Behavior in Service

Carbon and alloy steel thin hex nut — gb/t 6172.1 / iso 4035 (series 055) require a coating for corrosion protection. Zinc plating (with or without passivation) is the most common; hot-dip galvanizing is used for outdoor structural service; black-oxide is mainly a tarnish-prevention finish for tool-room use.

Comparable Grades

For Thin Hex Nut — GB/T 6172.1 / ISO 4035 (Series 055), class 8.8 is the comparable strength step. Move up when the joint preload approaches the proof load of the current class; move down when the joint is over-specified. For corrosion-critical service, switch to stainless A2 or A4.

Sizes of Thin Hex Nut — GB/T 6172.1 / ISO 4035 (Series 055) Available in Grade 12.9 Steel

SizePitch (mm)Width across flats s (mm)Width across corners e (mm)Nut height m (mm)Reference standard
M30.55.56.011.8ISO 4035 / GB/T 6172
M40.77.07.662.2ISO 4035 / GB/T 6172
M50.88.08.792.7ISO 4035 / GB/T 6172
M61.010.011.053.2ISO 4035 / GB/T 6172
M81.2513.014.384.0ISO 4035 / GB/T 6172
M101.516.017.775.0ISO 4035 / GB/T 6172
M121.7518.020.036.0ISO 4035 / GB/T 6172
M142.021.023.367.0ISO 4035 / GB/T 6172
M162.024.026.758.0ISO 4035 / GB/T 6172
M182.527.030.149.0ISO 4035 / GB/T 6172
M202.530.033.5310.0ISO 4035 / GB/T 6172
M243.036.039.9812.0ISO 4035 / GB/T 6172
M303.546.050.8515.0ISO 4035 / GB/T 6172
M364.055.060.7918.0ISO 4035 / GB/T 6172

Technical Drawing

Customize the parameters below — every spec field is editable, and the drawing redraws to match the values you choose. Changing the size will snap the other fields to that size's standard values; you can then override any individual value.

Sends the selected values to the quote form below.

Request a Quote

Adjust the parameters in the drawing above and click "Request this configuration" to send the exact specification straight to this form.

Request a Quotation

Specification
Business Information

Dimensions & Specifications (GB/T 6172.1 / ISO 4035)

SizePitch (mm)Width across flats s (mm)Width across corners e (mm)Nut height m (mm)Reference standard
M30.55.56.011.8ISO 4035 / GB/T 6172
M40.77.07.662.2ISO 4035 / GB/T 6172
M50.88.08.792.7ISO 4035 / GB/T 6172
M61.010.011.053.2ISO 4035 / GB/T 6172
M81.2513.014.384.0ISO 4035 / GB/T 6172
M101.516.017.775.0ISO 4035 / GB/T 6172
M121.7518.020.036.0ISO 4035 / GB/T 6172
M142.021.023.367.0ISO 4035 / GB/T 6172
M162.024.026.758.0ISO 4035 / GB/T 6172
M182.527.030.149.0ISO 4035 / GB/T 6172
M202.530.033.5310.0ISO 4035 / GB/T 6172
M243.036.039.9812.0ISO 4035 / GB/T 6172
M303.546.050.8515.0ISO 4035 / GB/T 6172
M364.055.060.7918.0ISO 4035 / GB/T 6172

Frequently Asked Questions

When should I move from class 12.9 to class 8.8 for Thin Hex Nut — GB/T 6172.1 / ISO 4035 (Series 055)?

Step up to class 8.8 when the joint preload approaches the proof load of the current class. The higher class adds preload at the same diameter, often saving size and weight.

Is Grade 12.9 Steel prone to hydrogen embrittlement?

Class 10.9 and above can be susceptible to hydrogen embrittlement when electroplated. Specify post-plating baking, or use mechanical-zinc / zinc-flake finishes which avoid the cathodic plating step.

Which finish is best for outdoor Thin Hex Nut — GB/T 6172.1 / ISO 4035 (Series 055)?

For outdoor service in steel, hot-dip galvanizing gives the longest life; zinc-flake (Geomet/Delta-Tone family) gives a thinner film with excellent salt-spray performance; standard zinc plating is the lowest-cost option for general indoor / shielded outdoor use.

What's the service temperature limit for Grade 12.9 Steel?

The practical service range is up to approx. +300 °C.

How do I request a quotation?

Use the technical drawing on this page to pick the exact configuration, then submit it with the quote form. We respond within one business day.