Grade 12.9 Steel Hex Nuts, Grade C

Grade 12.9 Steel Hex Nuts, Grade C reference image

Hex Nuts, Grade C manufactured in Grade 12.9 Steel (class 12.9) are dimensioned to ISO 4034. The sections below give the mechanical and physical properties of the grade, its behavior in corrosive and elevated-temperature service, and the full size table.

Why Choose Grade 12.9 Steel for Hex Nuts, Grade C

The highest common strength class, for high-load machine assembly. For hex nuts, grade c, this matters when requires plating or black-oxide protection is the primary requirement.

Mechanical & Physical Properties

Grade designationclass 12.9
Magnetic responseMagnetic
Service temperatureup to approx. +300 °C
Corrosion characteristicRequires plating or black-oxide protection

Corrosion Behavior in Service

Carbon and alloy steel hex nuts, grade c require a coating for corrosion protection. Zinc plating (with or without passivation) is the most common; hot-dip galvanizing is used for outdoor structural service; black-oxide is mainly a tarnish-prevention finish for tool-room use.

Comparable Grades

For Hex Nuts, Grade C, class 8.8 is the comparable strength step. Move up when the joint preload approaches the proof load of the current class; move down when the joint is over-specified. For corrosion-critical service, switch to stainless A2 or A4.

Sizes of Hex Nuts, Grade C Available in Grade 12.9 Steel

SizePitch (mm)Width across flats s (mm)Width across corners e min (mm)Nut height m (mm)Product gradeReference standard
M50.88.08.634.7Grade CISO 4034 / DIN 555
M61.010.010.895.2Grade CISO 4034 / DIN 555
M81.2513.014.26.8Grade CISO 4034 / DIN 555
M101.517.018.728.4Grade CISO 4034 / DIN 555
M121.7519.020.8810.8Grade CISO 4034 / DIN 555
M142.022.024.4912.8Grade CISO 4034 / DIN 555
M162.024.026.7514.8Grade CISO 4034 / DIN 555
M182.527.029.5615.8Grade CISO 4034 / DIN 555
M202.530.033.5318.0Grade CISO 4034 / DIN 555
M222.532.035.7219.4Grade CISO 4034 / DIN 555
M243.036.039.5521.5Grade CISO 4034 / DIN 555
M273.041.045.223.8Grade CISO 4034 / DIN 555
M303.546.050.8525.6Grade CISO 4034 / DIN 555
M364.055.060.7931.0Grade CISO 4034 / DIN 555
M424.565.071.334.0Grade CISO 4034 / DIN 555
M485.075.082.638.0Grade CISO 4034 / DIN 555

Technical Drawing

Customize the parameters below — every spec field is editable, and the drawing redraws to match the values you choose. Changing the size will snap the other fields to that size's standard values; you can then override any individual value.

Sends the selected values to the quote form below.

Request a Quote

Adjust the parameters in the drawing above and click "Request this configuration" to send the exact specification straight to this form.

Request a Quotation

Specification
Business Information

Dimensions & Specifications (ISO 4034)

SizePitch (mm)Width across flats s (mm)Width across corners e min (mm)Nut height m (mm)Product gradeReference standard
M50.88.08.634.7Grade CISO 4034 / DIN 555
M61.010.010.895.2Grade CISO 4034 / DIN 555
M81.2513.014.26.8Grade CISO 4034 / DIN 555
M101.517.018.728.4Grade CISO 4034 / DIN 555
M121.7519.020.8810.8Grade CISO 4034 / DIN 555
M142.022.024.4912.8Grade CISO 4034 / DIN 555
M162.024.026.7514.8Grade CISO 4034 / DIN 555
M182.527.029.5615.8Grade CISO 4034 / DIN 555
M202.530.033.5318.0Grade CISO 4034 / DIN 555
M222.532.035.7219.4Grade CISO 4034 / DIN 555
M243.036.039.5521.5Grade CISO 4034 / DIN 555
M273.041.045.223.8Grade CISO 4034 / DIN 555
M303.546.050.8525.6Grade CISO 4034 / DIN 555
M364.055.060.7931.0Grade CISO 4034 / DIN 555
M424.565.071.334.0Grade CISO 4034 / DIN 555
M485.075.082.638.0Grade CISO 4034 / DIN 555

Frequently Asked Questions

What corrosion resistance do Grade 12.9 Steel Hex Nuts, Grade C offer?

Grade 12.9 Steel Hex Nuts, Grade C provide requires plating or black-oxide protection with a service range of up to approx. +300 °C.

When should I move from class 12.9 to class 8.8 for Hex Nuts, Grade C?

Step up to class 8.8 when the joint preload approaches the proof load of the current class. The higher class adds preload at the same diameter, often saving size and weight.

Is Grade 12.9 Steel prone to hydrogen embrittlement?

Class 10.9 and above can be susceptible to hydrogen embrittlement when electroplated. Specify post-plating baking, or use mechanical-zinc / zinc-flake finishes which avoid the cathodic plating step.

Which finish is best for outdoor Hex Nuts, Grade C?

For outdoor service in steel, hot-dip galvanizing gives the longest life; zinc-flake (Geomet/Delta-Tone family) gives a thinner film with excellent salt-spray performance; standard zinc plating is the lowest-cost option for general indoor / shielded outdoor use.