Grade 8.8 Steel Turnbuckle — ISO / DIN (Series 156)

For Turnbuckle — ISO / DIN (Series 156) in Grade 8.8 Steel, the controlling decisions are corrosion, strength and service temperature. This guide summarizes those three for Grade 8.8 Steel Turnbuckle — ISO / DIN (Series 156) and lists every size we supply.

Why Choose Grade 8.8 Steel for Turnbuckle — ISO / DIN (Series 156)

The workhorse medium-carbon alloy grade for structural joints. For turnbuckle — iso / din (series 156), this matters when requires plating (zinc) for corrosion protection is the primary requirement.

Mechanical & Physical Properties

Grade designationclass 8.8
Magnetic responseMagnetic
Service temperatureup to approx. +300 °C
Corrosion characteristicRequires plating (zinc) for corrosion protection

Corrosion Behavior in Service

Carbon and alloy steel turnbuckle — iso / din (series 156) require a coating for corrosion protection. Zinc plating (with or without passivation) is the most common; hot-dip galvanizing is used for outdoor structural service; black-oxide is mainly a tarnish-prevention finish for tool-room use.

Galvanic & Galling Considerations

For turnbuckle — iso / din (series 156) in steel, the dominant compatibility issue is hydrogen embrittlement at high property classes (10.9 and above) when electroplated. Plating must be followed by an appropriate baking treatment, or a non-electroplated finish (mechanical zinc, zinc flake) should be substituted.

Sizes of Turnbuckle — ISO / DIN (Series 156) Available in Grade 8.8 Steel

Thread sizeTotal length closed (mm)Take-up length (mm)Working load limit (kg)MaterialReference standard
M61057580Drop-forged steel, hot-dip galvanizedDIN 1480 / GB/T 5973
M812590140Drop-forged steel, hot-dip galvanizedDIN 1480 / GB/T 5973
M10150110230Drop-forged steel, hot-dip galvanizedDIN 1480 / GB/T 5973
M12180135340Drop-forged steel, hot-dip galvanizedDIN 1480 / GB/T 5973
M16230170700Drop-forged steel, hot-dip galvanizedDIN 1480 / GB/T 5973
M202902151200Drop-forged steel, hot-dip galvanizedDIN 1480 / GB/T 5973
M243552601800Drop-forged steel, hot-dip galvanizedDIN 1480 / GB/T 5973
M304203203200Drop-forged steel, hot-dip galvanizedDIN 1480 / GB/T 5973

Technical Drawing

Customize the parameters below — every spec field is editable, and the drawing redraws to match the values you choose. Changing the size will snap the other fields to that size's standard values; you can then override any individual value.

Sends the selected values to the quote form below.

Request a Quote

Adjust the parameters in the drawing above and click "Request this configuration" to send the exact specification straight to this form.

Request a Quotation

Specification
Business Information

Dimensions & Specifications (ISO / DIN)

Thread sizeTotal length closed (mm)Take-up length (mm)Working load limit (kg)MaterialReference standard
M61057580Drop-forged steel, hot-dip galvanizedDIN 1480 / GB/T 5973
M812590140Drop-forged steel, hot-dip galvanizedDIN 1480 / GB/T 5973
M10150110230Drop-forged steel, hot-dip galvanizedDIN 1480 / GB/T 5973
M12180135340Drop-forged steel, hot-dip galvanizedDIN 1480 / GB/T 5973
M16230170700Drop-forged steel, hot-dip galvanizedDIN 1480 / GB/T 5973
M202902151200Drop-forged steel, hot-dip galvanizedDIN 1480 / GB/T 5973
M243552601800Drop-forged steel, hot-dip galvanizedDIN 1480 / GB/T 5973
M304203203200Drop-forged steel, hot-dip galvanizedDIN 1480 / GB/T 5973

Frequently Asked Questions

Can Grade 8.8 Steel replace stainless steel structurally?

No — stainless A2/A4 cannot match class 10.9 / 12.9 strength. Stainless is selected for corrosion, not raw strength.

Are Grade 8.8 Steel Turnbuckle — ISO / DIN (Series 156) magnetic?

Grade 8.8 Steel Turnbuckle — ISO / DIN (Series 156) are magnetic.

What corrosion resistance do Grade 8.8 Steel Turnbuckle — ISO / DIN (Series 156) offer?

Grade 8.8 Steel Turnbuckle — ISO / DIN (Series 156) provide requires plating (zinc) for corrosion protection with a service range of up to approx. +300 °C.

When should I move from class 8.8 to class 10.9 / 12.9 for Turnbuckle — ISO / DIN (Series 156)?

Step up to class 10.9 / 12.9 when the joint preload approaches the proof load of the current class. The higher class adds preload at the same diameter, often saving size and weight.

How do I request a quotation?

Use the technical drawing on this page to pick the exact configuration, then submit it with the quote form. We respond within one business day.